Phase | Ingredient | %W/W |
---|---|---|
A1 | DI Water | 70.000 |
A2 | Carbopol Ultrez-21 (Lubrizol (Protameen)) | 0.250 |
B1 | Protacide NA2-P (Protameen) | 0.050 |
B2 | dl-Panthenol (Protameen) | 0.200 |
B3 | Glycerin, 99% (Protameen) | 2.000 |
C1 | Anhydrous Protalan (Protameen) | 1.500 |
C2 | Protachem HCO-40 (Protameen) | 1.000 |
C3 | Protalan Wax (Protameen) | 18.000 |
C4 | Protachem CS-50 (Protameen) | 4.000 |
C5 | Shea Butter | 0.500 |
D1 | Fixate Design Polymer (Lubrizol (Protameen)) | 1.000 |
D2 | Triethanolamine | qs |
D3 | Preservative | qs |
D4 | Fragrance | qs |
Total | 100.000 |
1. Meter DI Water (A1) into main tank, sprinkle Carbopol Ultrez-21 (A2) on top, allow to self-wet (with no agitation).
2. Once Phase A is completely wetted out, begin propeller agitation of batch, add Phase B ingredients one at a time. Begin heating to 75-80°C.
3. In auxiliary tank, combine all ingredients of Phase C, mix and heat 75-80°C, until homogenous.
4. Once both phases are homogeneous, slowly add Phase C into main tank with Phase AB.
5. Mix until homogeneous, being careful not to aerate the batch.
6. Remove from heat, begin cooling to 50-55°C
7. Add Fixate Design Polymer (D1) to main
8. Add Triethanolamine (D2) to neutralise batch
9. Add Preservative (D3)
10. Add Fragrance (D4)